Add to Cart
Plastic bottle blowing machine/ Semi-Automatic Bottle Blow Moulding Machine/ PET bottle making
Full automatic blow molding machine is suitable for producing PET plastic containers and bottles in all shapes . it is widely used to produce the carbonated bottle,mineral water bottle, pesticide bottle,oil bottle,cosmetics bottle ect.
Reasonable design , full automaticlly control, save power and labor.
Adopting high quality components.
Feeding system carries the preforms by robot arms automatically.
Infrared oven adopts the quartz lamp to heat the PET tube.
Full automatic process with low investment,high efficiency , quick and safe for operating,easy for maintenance
Setup for automatic used pet bottle blowing machine
Full automatic blowing molding machine
Pneumatic part: 1. Valve 2. Cylinder 3 Brand: SMC
Electric part: 1. PLC 2. Operating system: 3. Brand: LG 1. Relay: OMRON
Note: All of the electrical components adopt CE, UL, CCC approved international advanced high-tech product.
Full automatic blow molding machine is suitable for producing PET plastic containers and bottles in all shapes.
It is widely used to produca the carbonated bottle,mineral water,pesticide bottle,oil bottle,cosmetics bottle, wide-mouth bottle ect.
Defects | Causes | Solutions |
Pearly luster appears on the product and the gate part on the bottom deviates the center | 1The heating temperature for the pre-form is too low | Raise heating temperature |
2Blowing time is too early | Prolong the blowing time | |
3Heating of pre-form is not uniformed | Check if the rotating electric motor of the oven works | |
4The linear velocity for pulling pre-form is too low | Raise working pressure flux of pre-forms | |
The product can’t be formed | 1 Insufficient pressure | Raise pressure |
2Insufficient blowing flux | Raise blowing flux | |
3Stretching rate is too high | Redesign stretching rate | |
4Blowing valve is damaged | Replace the valve | |
Wall thickness of products is not uniform | 1Wall thickness of pre-forms is not uniform | Replace pre-forms |
2Stretching rate is too low | Redesign stretching rate | |
The neck of the product shrinks into a loop | Blow time is too late | Advance blowing time |
The bottom of the product does not form or is too thick | 1Blow time is too late | Advance blowing time
|
2 Heating temperature on the bottom of pre-forms is too low | Raise corresponding heating temperature | |
Transparency of products is not good | 1The pre-form is not transparent enough | The plastic material is not dry enough |
2The second-time heating temperature for the pre-form is too high | Reduce the heating temperature and heating time | |
3There is moisture in the blowing air | Check if filter outlet is obstructed. |